What is nylon fabric?
Nylon spinning, also known as nylon spinning, is nylon Spun silk fabric made of filament. It has the characteristics of smooth and fine texture, smooth silk surface, soft hand feel, light weight but strong and wear-resistant, bright color, easy to wash and quick-drying, etc. It is mainly used as a fabric for men’s and women’s clothing. The fabric weave is plain weave, and the change weave is rhombus lattice, nylon hexagonal lattice, and nylon Oxford lattice.
Features
1. Nylon is made of nylon (see Poly
Amide fiber) filament woven textile, also known as nylon textile. fine surface
It is clean and smooth, with tough texture, good elasticity and strength. It is a material used for making clothing and high-end decorative packaging. After coating, it can be made into ski jackets, raincoats, umbrellas, etc. There are two types of nylon spun, thin and thick. The thin weight is about 40g/m2, and the warp and weft yarns are average.
A single 30-denier nylon yarn is used; the thick type weighs about 80g/m2, and a single 70-denier nylon yarn is used for the warp and weft yarns.
2. Nylon spinning warp and weft do not need to be twisted. The raw silk needs to be refined, dyed or printed, and heat-set. The thermoplasticity of nylon yarn can also be used to roll various patterns and wrinkles. There are many ways to post-process nylon spun silk. Some can be refined, dyed or printed; some can be calendered or embossed; some can be coated.
3. Nylon spun by fabric whitening, fabric dyeing, fabric printing, fabric calendering, and fabric embossing, the fabric is smooth and dense, and the silk surface is smooth , soft to the touch, light and durable, bright in color, easy to wash and quick to dry.
Processing and processing
About Nisi Spun Several key points in pre-treatment: the efficiency of removing PAC, the formulation of the desizing process; the removal of oil and other impurities, the selection of chelating agents in the desizing process; if the desizing efficiency is above 95%, the dyeing process Level dyeing is not a big problem, but the presence of heavy metal ions in the water quality will also affect the dyeing quality. It is recommended to use an acidic regulator with a certain chelating function and prevent the existence of residual slurry. To solve these problems, the dyeing quality will be improved. Guaranteed!
There are many ways to post-process nylon spun silk. Some can be refined, dyed or printed; some can be calendered or embossed; some can be calendered or embossed; Can be coated.
Identification
When nylon burns, one side It melts and burns slowly on one side. There is no smoke or slight white smoke when burning, and the flame is very little and blue. Has a celery aroma. Gray is a light brown hard lump that is not easy to crush.
The difference between polyester taffeta, pongee, nylon and taslan
1. From the raw materials:
Darkmode is 100% polyester is used for lining; pongee is also 100% polyester, with many low-grade varieties; nylon is what we call nylon cloth and is made of nylon; Taslon is also an all-nylon yarn textile cloth .
2. From the weaving method:
Polyester taffeta and nylon fabricThe method is the same, it is a one-up-down weaving method.
Taslan’s weaving method is one up and down, but its warp direction is particularly thick, at least than its weft direction. 1x thicker. Taslon in cotton is called grosgrain.
The weaving method of pongee is roughly the same as polyester taffeta. This is not easy to distinguish, but it can be easily distinguished from other methods below. Easy to distinguish.
3. From the feel:
Polyester taffeta and nylon are similar, with pongee feeling very soft and Taslon feeling very astringent.
When comparing, use the fabric burning method, first separate nylon and polyester, nylon belongs to Taslan and nylon; polyester It belongs to polyester taffeta and pongee; needless to say, nylon taffeta and taslan, but the difference between polyester taffeta and pongee is different in feel. The most important thing is “split”. Polyester taffeta When tearing, its torn edge and both sides will have deep splits, but pongee does not. When not tearing the cloth, you can pull it along the warp direction of the cloth to both sides. With a little force, the polyester taffeta will break. There will be “splits”, but pongee will not.